Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUMIPLAS LD590T Light diffusion ABS Description: Extrusion, Light diffusion, High ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL GP3202Z PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | DIN 53452; ASTM D790 |
Kolon NOPLA® KE131 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Samyang Trirex® TH3022N Polycarbonate, High Flow Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.TH3022N is a high flow, flame retardant grade.Applications: LCD TV, Laptop and Monitor.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |