Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.80 GPa | 1420 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Flexural Modulus | 9.79 GPa | 1420 ksi | ASTM D790 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN133G43SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Flexural Modulus | 9.82 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 9.80 GPa @Temperature 100 °C |
1420 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.79 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 LNP THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 9.80 GPa @Temperature 100 °C |
1420 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Modulus | 9.77 GPa | 1420 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.79 GPa | 1420 ksi | ASTM D790 |
PlastxWorld CEVIAN® B5726 30% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ASTM D790 |
Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Improved surface appearance gradeAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178-93 |
Wellman Wellpet® GF100-BK1 PET, 30% Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178-93 |
Wellman Wellpet® GF100-N1 30% Glass Fiber Reinforced, Natural PET Description: Glass Fiber Reinforced, Natural PETInformation provided by Wellman. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ASMT D790 |
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ASTM D790 |
Toyobo Vylopet® EMC130-04 Glass Reinforced Polyester, Easy Molding Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking r.. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178 |
Polyram PlusTek RA314G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized 50% Glass fiber reinforced, heat stabilized Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | dry; ISO 178 |
DSM Novamid® 1015GH35 BK37 PA6-GF35 35% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |