| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 9.80 GPa | 1420 ksi | STN EN ISO 178 |
| Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
| Flexural Modulus | 9.79 GPa | 1420 ksi | ASTM D790 |
| Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | |
| Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
| Kolon KOPET® KP133G45 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | 1.3 mm/min; ASTM D790 |
| Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ASTM D790 |
| Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
| Flexural Modulus | 9.80 GPa @Temperature 100 °C |
1420 ksi @Temperature 212 °F |
ISO 178 |
| Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
| Flexural Modulus | 9.77 GPa | 1420 ksi | ISO 178 |
| SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific) LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
| Flexural Modulus | 9.79 GPa | 1420 ksi | ASTM D790 |
| SABIC Innovative Plastics LNP STAT-KON DE004 PC LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® T102G30 PET, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D638 |
| Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 9.79 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 LNP THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.77 GPa | 1420 ksi | ISO 178 |
| SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
| Flexural Modulus | 9.79 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
| Flexural Modulus | 9.78 GPa | 1420 ksi | ISO 178 |
| SABIC Innovative Plastics LNP VERTON WV006 PBT (Europe-Africa-Middle East) LNP VERTON* WV006 is a compound based on Polybutylene Terephalate resin containing Long Glass. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ASTM D790 |
| Plenco 3509 Phenolic, Granular, Transfer Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ASTM D790 |
| Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178-93 |
| Wellman Wellpet® GF100-BK1 PET, 30% Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178-93 |
| Wellman Wellpet® GF100-N1 30% Glass Fiber Reinforced, Natural PET Description: Glass Fiber Reinforced, Natural PETInformation provided by Wellman. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ASMT D790 |
| Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ASTM D790 |
| Plenco 4504 Phenolic, Granular, Compression Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | dry; ISO 178 |
| DSM Novamid® 1015G35 NAT PA6-GF35 35% Glass Reinforced, Injection Molding |
|||
| Flexural Modulus | 9.79 GPa | 1420 ksi | ASTM D790 |
| Clariant Renol PA2SP0006 Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
| Flexural Modulus | 9.80 GPa | 1420 ksi | ISO 178 |
| Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
| Flexural Modulus | 9.78 GPa | 1420 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||