Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 10% Glass Fiber Reinforced
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 167 MPa
24200 psi
5 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
5 mm/min; ASTM D638
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Flexural Modulus 9.81 GPa
1420 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.637 J/cm

@Thickness 3.17 mm
1.19 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 290 °C

@Thickness 6.40 mm
554 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 HB

@Thickness 0.400 - 3.00 mm
HB

@Thickness 0.0157 - 0.118 in