| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
| Kolon SPESIN® KP213G45 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
| Kolon KOPA® KN133G43SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
| Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | DIN 53452; ASTM D790 |
| Kolon KOPET® KP133G45 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
| Flexural Modulus | 9.81 GPa @Thickness 3.20 mm |
1420 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | |
| Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Window Strip SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® T102G30 PET, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D638 |
| Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | 2.8 mm/min; ASTM D638 |
| Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10 LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
| Flexural Modulus | 9.81 GPa | 1420 ksi | ASTM D790 |
| LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||