Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
Nylene® PA6 Glass Filled 5233 HS Nylon 6 33% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 9.30 GPa @Temperature 23.0 °C |
1350 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2mm/min; ASTM D790 |
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an.. |
|||
Flexural Modulus | 9.32 GPa | 1350 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333G33BL G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 9.28 GPa | 1350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer LNP* LUBRICOMP* KFL36 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66 LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by .. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFL26S PA 66 (Asia Pacific) LNP* Lubricomp* RFL26S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 ML5 HS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 ML5 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and He.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/30/TF/15 BK223 PA66 |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/30/TF/22 BK223 PA66 |
|||
Flexural Modulus | 9.32 GPa | 1350 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.32 GPa | 1350 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OF008G PPS - LINEAR LNP* THERMOCOMP* OF008G is a compound based on PPS - Linear containing 15% Glass Fiber, 25% Milled Glass. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178-93 |
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830LS-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced and heat stabilized Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 t.. |