Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 MF40 Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact Modified and Semi ConductiveAppearance: Black.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill FR® TPX-PBT-01006 40% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 40% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM L NAT002 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/30/TF/15 RED PA66 |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/30/TF/22 BK223 PA66 |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL NC220 PPE+HIPS (Asia Pacific) |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133L (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthForm: PelletsApplications: Automotive under the hoodInformation provided b.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D570 |
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled
(discontinued **) XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o.. |