Material Notes:
LNP* Lubricomp* RFL26S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Flexural Strength 275 MPa
39900 psi
ASTM D790
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.21 J/cm
21.00 ft-lb/in
ASTM D4812
Coefficient of Friction, Dynamic 0.66
0.66
ASTM D3702 Modified
Coefficient of Friction, Static 0.57
0.57
ASTM D3702 Modified
K (wear) Factor 10.1 x 10-8 mm³/N-M
5.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 253 °C

@Thickness 3.20 mm
487 °F

@Thickness 0.126 in
unannealed; ASTM D648