Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 LNP* LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66 LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66 LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan.. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific) LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXY PA 66 LNP* Thermocomp* RF006XXY is a compound based on Nylon 66 containing 30% Glass Fiber. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 LNP THERMOCOMP* PF006S is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 LNP THERMOCOMP* PF006U is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of thie grade are: UV Stabilized. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific) LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |