Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® IP300 PC Improved toughness/impact strength at ambient/low temperatures for automotive instrument panels, knee bolsters and trim. Range gray and black only.This data was supplied by SABIC-IP for the America.. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7647 PC Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Plenco 4224 Phenolic, Granular, Transfer Molded
(discontinued **) Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive ap.. |
|||
Flexural Yield Strength | 84.1 - 290 MPa | 12200 - 42000 psi | Average value: 198 MPa Grade Count:36 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 84.3 MPa @Thickness 3.20 mm |
12200 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RX93237 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX93237 is a compound based on Nylon 66 resin containing PTFE, Silicone, MOS2. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 195HP PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Asia Pacific) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 5220 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 6200 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 6600 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Covestro Bayblend® 2253 Polycarbonate + ABS Blend, Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Spartech APET SP4110 Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | ASTM D790 |
E-Polymers Tekaloy® G70A2 Impact Resistance, Easy Molding PC/ABS Alloy Impact Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |