| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PETG Copolyester |
| Manufacturer | Spartech |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Spartech PETG 3D Lenticular 3-D Specialty Sheet.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 106 | 106 | ASTM D2240 |
| Tensile Strength at Break | 57.9 MPa | 8400 psi | ASTM D882 |
| Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D882 |
| Elongation at Break | 300 % | 300 % | ASTM D882 |
| Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D882 |
| Flexural Yield Strength | 84.1 MPa | 12200 psi | ASTM D790 |
| Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
| Izod Impact, Unnotched | 0.497 J/cm | 0.930 ft-lb/in | ASTM D256 |
| 0.278 J/cm @Temperature -40.0 °C |
0.520 ft-lb/in @Temperature -40.0 °F |
ASTM D256 | |
| Falling Dart Impact | 678 J | 500 ft-lb | 73°F; ASTM D1709A |
| 542 J @Temperature -40.0 °C |
400 ft-lb @Temperature -40.0 °F |
ASTM D1709A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 57.6 µm/m-°C @Temperature 20.0 °C |
32.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D540 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 90 % | 90 % | Gardner; ASTM D2523 |