Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.50 GPa | 943 ksi | |
Plastcom SLOVAMID 6 GF 15 FRG 2 LW PA6, 15% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 960°.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | |
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 HS-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 SG-GV 1515 Nylon 6.6 for injection molding, 15% mineral filled and 15% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL B63 SG-GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® SF 2230 Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 1mm/min; ISO 527 |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-2/5 |
Styron INSPIREâ„¢ DLGF 9621.00 Compounded Polypropylene, 60% LGF Overview: DLGF 9621.00 is a polypropylene homopolymer reinforced with 60% by weight of long glass fiber. PP-LGF60, Long Glassfiber Granulate). DLGF 9621.00 is produced by pultrusion/melt-impregnatio.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-2/5 |
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding... |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BM-30 PA6-MD30 Product description: Grilon BM-30 is a 30% mineral reinforced PA6 injection moulding grade. Grilon BM-30 has the following important properties: heat stabilizedimpact resistantisotropic shrinkagelig.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black Information provided by Eurotec® |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 Information provided by Eurotec® |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | |
BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced Glass fiber reinforced grade containing halogen-free flame-retardant; for moldings with high heat resistance and stiffness (e.g. relay parts, controller and switch housings).Data was collected by IS.. |
|||
Tensile Modulus | 6.50 GPa @Treatment Temp. 70.0 °C, Time 1.44e+6 sec |
943 ksi @Treatment Temp. 158 °F, Time 400 hour |
62% rel. humidity |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ASTM D638 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |