Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw material used is sebacic acid, synthesized from castor oil which is obtained from the seeds of Ricinus communis, the castor oil plant. From a technical standpoint, AKROMID® S closes the gap between PA 6/PA 6.6 and PA 12. It is characterized by significantly lower moisture absorption compared to PA 6 and PA 6.6. At 23 °C and 50 % relative humidity, typical values for these product types are 3 % and 2.8 %, respectively. With a value of approximately 1.4 %, PA 6.10 absorbs just half as much moisture and can therefore be used as an engineering material in applications requiring a high dimensional consistency. Moreover, it exhibits excellent cold impact resistance. Other outstanding characteristics include very good chemical resistance due to the structure of the polymer and high hydrolysis resistance, although it can be processed like all common polyamides. The materials from the PA 6.10 product family are further characterized by exceptional dimensional stability, good surface resistance, good abrasion resistance and wear behaviour, and an improved carbon footprint. This is due to the fact that the plant-based raw materials have already removed CO2 from the environment during their growth phase. The product portfolio currently comprises one non reinforced variant and several reinforced variants with a glass-fibre content ranging from 15 % to 50 %. AKROMID® S is a bioplastic according to today’s standards. Unlike certain materials used in the packaging industry, however, the material is not biodegradable. The distinguishing feature of AKROMID® S is its reduced ecological footprint: The use of harmful CO2 per ton of polyamide produced from renewable resources is significantly lower compared to one ton produced from fossil-based resources, without affecting the product’s performance characteristics.Applications:Automotive SectorConnectors and housingsNon-return valvesPower steering-fluid reservoirsCorrugated tubing and fluid pipesMachine Construction and Tool-BuildingGearsDoor handles and fittingsOffice equipment, housings, functional parts, amongst othersConnectors and plugsPower toolsSports and LeisureComponents in high-end garden toolsBicycle accessoriesSail-boat accessoriesWinter sports accessoriesInformation from Akro-Plastic
Physical Properties Metric English Comments
Density 1.31 g/cc

@Temperature 23.0 °C
0.0473 lb/in³

@Temperature 73.4 °F
ISO 1183
Filler Content 30 %
30 %
ISO 1172
Water Absorption 1.2 %

@Temperature 70.0 °C
1.2 %

@Temperature 158 °F
62% r.h., Humdity; ISO 62
Water Absorption at Saturation 0.40 %

@Temperature 25.0 °C,
Treatment Temp. 70.0 °C
0.40 %

@Temperature 77.0 °F,
Treatment Temp. 158 °F
62% rel. humidity
0.60 %

@Temperature 45.0 °C,
Treatment Temp. 70.0 °C
0.60 %

@Temperature 113 °F,
Treatment Temp. 158 °F
62% rel. humidity
0.70 %

@Temperature 70.0 °C,
Treatment Temp. 70.0 °C
0.70 %

@Temperature 158 °F,
Treatment Temp. 158 °F
62% rel. humidity
1.0 %

@Treatment Temp. 70.0 °C,
Temperature 160 °C
1.0 %

@Treatment Temp. 158 °F,
Temperature 320 °F
62% rel. humidity
1.1 %

@Treatment Temp. 70.0 °C,
Temperature 240 °C
1.1 %

@Treatment Temp. 158 °F,
Temperature 464 °F
62% rel. humidity
1.2 %

@Treatment Temp. 70.0 °C,
Temperature 340 °C
1.2 %

@Treatment Temp. 158 °F,
Temperature 644 °F
62% rel. humidity
1.2 %

@Treatment Temp. 70.0 °C,
Temperature 400 °C
1.2 %

@Treatment Temp. 158 °F,
Temperature 752 °F
62% rel. humidity
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4
Spiral Flow 40.0 cm
15.7 in
AKRO
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
5 [mm/min]; ISO 527-1/2
Elongation at Break 4.5 %
4.5 %
5 [mm/min]; ISO 527-1/2
5.5 %
5.5 %
2 [mm/min], Flexural; ISO 178
Tensile Modulus 8.60 GPa
1250 ksi
1[mm/min]; ISO 527-1/2
6.50 GPa

@Treatment Temp. 70.0 °C,
Time 1.44e+6 sec
943 ksi

@Treatment Temp. 158 °F,
Time 400 hour
62% rel. humidity
6.70 GPa

@Treatment Temp. 70.0 °C,
Time 1.22e+6 sec
972 ksi

@Treatment Temp. 158 °F,
Time 340 hour
62% rel. humidity
6.90 GPa

@Treatment Temp. 70.0 °C,
Time 864000 sec
1000 ksi

@Treatment Temp. 158 °F,
Time 240 hour
62% rel. humidity
7.00 GPa

@Treatment Temp. 70.0 °C,
Time 576000 sec
1020 ksi

@Treatment Temp. 158 °F,
Time 160 hour
62% rel. humidity
7.90 GPa

@Treatment Temp. 70.0 °C,
Time 270000 sec
1150 ksi

@Treatment Temp. 158 °F,
Time 75.0 hour
62% rel. humidity
8.00 GPa

@Treatment Temp. 70.0 °C,
Time 180000 sec
1160 ksi

@Treatment Temp. 158 °F,
Time 50.0 hour
62% rel. humidity
8.20 GPa

@Treatment Temp. 70.0 °C,
Time 90000 sec
1190 ksi

@Treatment Temp. 158 °F,
Time 25.0 hour
62% rel. humidity
Flexural Strength 230 MPa
33400 psi
2 [mm/min]; ISO 178
Flexural Modulus 7.70 GPa
1120 ksi
2 [mm/min]; ISO 178
Izod Impact, Unnotched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
After 200 hours in ZnCl<sub>2</sub>
Charpy Impact Unnotched 10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 11357-1, DSC,10 [K/min]
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
HDT/A; ISO 75-1/2
Deflection Temperature at 8.0 MPa 145 °C
293 °F
HDT/C; ISO 75-1/2
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Processing Properties Metric English Comments
Feed Temperature 60.0 - 80.0 °C
140 - 176 °F
Nozzle Temperature 240 - 295 °C
464 - 563 °F
Zone 1 220 - 300 °C
428 - 572 °F
Zone 2 220 - 300 °C
428 - 572 °F
Zone 3 220 - 300 °C
428 - 572 °F
Zone 4 220 - 300 °C
428 - 572 °F
Melt Temperature 260 - 310 °C
500 - 590 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 80.0 °C
176 °F
Dry Time <= 4 hour
<= 4 hour
Hold Pressure 30.0 - 80.0 MPa
4350 - 11600 psi
Back Pressure 5.00 - 15.0 MPa
725 - 2180 psi
Descriptive Properties Value Comments
Rate acc. FMVSS 302 ( Passed
Rate acc. FMVSS 302,( FMVSS 302, >1 [mm] Thickness
Users viewing this material also viewed the following: