Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.70 GPa | 537 ksi | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | Result based on similar products; ISO 527 |
Victrex® PEEK 600PF Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Manifattura Cattaneo PET Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® SAN C Injection Molding Grade |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East) VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-2 |
Styron TYRILâ„¢ 875 SAN Resin Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1013GMF H2 NAT/BK37 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding, Excellent Dimensional Stability |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AS/2 PA66 Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BS V0 PA6 Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties: Halogen and phosphorous-f.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 5004 (BM-30/2 UV) PA666-MD30 Product description: Grilon XE 5004 is a normal viscosity PA6 injection molding grade with 30% mineral reinforcement, which is additionally UV stabilized. Grilon XE 5004 has the following important .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
Styrolution Luran® 368 R SAN General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |