Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® AS/2 PA66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 is used typically in applications such as cable ties, clamps, handles, spectacle frames, and furniture components.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
150 MPa
21800 psi
dry; ISO 2039-1
Tensile Strength at Break 80.0 MPa
11600 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 60.0 MPa
8700 psi
conditioned; ISO 527-1/-2
95.0 MPa
13800 psi
dry; ISO 527-1/-2
Elongation at Break 10 %
10 %
dry; ISO 527-1/-2
10 %
10 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
12 %
12 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.70 GPa
247 ksi
conditioned; ISO 527-1/-2
3.70 GPa
537 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
1.20 J/cm²
5.71 ft-lb/in²
conditioned; ISO 179/1eA
0.400 J/cm²

@Temperature 30.0 °C
1.90 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.400 J/cm²

@Temperature 30.0 °C
1.90 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
29.0 kV/mm
737 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Hydraulic systems
Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Nucleated