| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 | 
| Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | Test Condition: 150x105x3; acc. ISO 2577 | 
| Melt Flow |           23           g/10 min           @Load 10.0 kg, Temperature 220 °C  | 
                  23           g/10 min           @Load 22.0 lb, Temperature 428 °F  | 
        ISO 1133 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Elongation at Break | 3.2 % | 3.2 % | 50 mm/min; ISO 527-1,-2 | 
| Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527-1,-2 | 
| Flexural Strength | 111 MPa | 16100 psi | 2 mm/min; ISO 178 | 
| Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 | 
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | ISO 180-1A | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ISO 75-1,-2 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 214 °F | ISO 75-1,-2 | 
| Vicat Softening Point |           104           °C           @Load 5.10 kg  | 
                  219           °F           @Load 11.2 lb  | 
        50°C/hour; ISO 306 | 
| Flammability, UL94 |           HB                     @Thickness 1.60 mm  | 
                  HB                     @Thickness 0.0630 in  |