| Category | Polymer , Thermoplastic , Polyimide, Thermoplastic |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Duratron® PI |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183-1 |
| Moisture Absorption at Equilibrium | 2.2 % | 2.2 % | 50% RH |
| Water Absorption at Saturation | 4.0 % | 4.0 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell E | 95 | 95 | ISO 2039-2 |
| Hardness, Shore D | 90 | 90 | |
| Ball Indentation Hardness | 235 MPa | 34100 psi | ISO 2039-1 |
| Tensile Strength | 115 MPa | 16700 psi | at Break (NYP); ISO 527-1/-2 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1/-2 |
| Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-1/-2 |
| Flexural Strength | 185 MPa | 26800 psi | |
| Compressive Strength | 35.0 MPa @Strain 1 % |
5080 psi @Strain 1 % |
ISO 604 |
| 69.0 MPa @Strain 2 % |
10000 psi @Strain 2 % |
ISO 604 | |
| 145 MPa @Strain 5 % |
21000 psi @Strain 5 % |
ISO 604 | |
| K Factor (ISO) | 12 µm/km | 12 µm/km | |
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179-1/1eU |
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179-1/1eA |
| Coefficient of Friction, Dynamic | 0.30 - 0.50 | 0.30 - 0.50 | |
| Limiting Pressure Velocity | 0.380 MPa-m/sec | 10800 psi-ft/min | at 1 m/s unlubricated |
| 1.04 MPa-m/sec | 29700 psi-ft/min | at 0.1 m/s unlubricated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 40.0 µm/m-°C @Temperature 23.0 - 100 °C |
22.2 µin/in-°F @Temperature 73.4 - 212 °F |
|
| Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 240 °C | 464 °F | Continuous |
| Deflection Temperature at 1.8 MPa (264 psi) | 355 °C | 671 °F | ISO 75-1/-2 |
| Glass Transition Temp, Tg | 365 °C | 689 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 51 % | 51 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.4 @Frequency >=100000 Hz |
3.4 @Frequency >=100000 Hz |
IEC 60250 |
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
| Dissipation Factor | 0.0060 @Frequency 100000 Hz |
0.0060 @Frequency 100000 Hz |
IEC 60250 |
| Comparative Tracking Index | 125 V | 125 V | IEC 60112 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| European Food 1935/2004 | No | No | |
| FDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |