Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG38U ABS High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | ISO 180/1A |
Dow INSPIRE™ D7030EZ Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Izod Impact, Notched (ISO) | 27.0 - 176 kJ/m² | 12.8 - 83.7 ft-lb/in² | Average value: 75.7 kJ/m² Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East) LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | ASTM D256 |
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature -50.0 °C |
12.8 ft-lb/in² @Temperature -58.0 °F |
|
Dow LDPE 4012M Low Density Polyethylene DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge.. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermotuf V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific) LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |
|||
Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |