| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP VERTON |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP VERTON RX00327 PA 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
| Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.690 % | 0.690 % | 50% RH, 24 hrs; ASTM D570 |
| 1.00 % | 1.00 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm @Time 86400 sec |
0.0060 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 206 MPa | 29900 psi | 5 mm/min; ISO 527 |
| 208 MPa | 30200 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 206 MPa | 29900 psi | 5 mm/min; ISO 527 |
| 208 MPa | 30200 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 2.0 % | 2.0 % | Type I, 5 mm/min; ASTM D638 |
| 2.0 % | 2.0 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 2.0 % | 2.0 % | Type I, 5 mm/min; ASTM D638 |
| 2.0 % | 2.0 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 14.74 GPa | 2138 ksi | 1 mm/min; ISO 527 |
| 15.24 GPa | 2210 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 291 MPa | 42200 psi | ISO 178 |
| 297 MPa | 43100 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Yield Strength | 297 MPa | 43100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 11.9 GPa | 1730 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 11.91 GPa | 1727 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 2.39 J/cm | 4.48 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 10.9 J/cm | 20.4 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 67.0 kJ/m² | 31.9 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 77.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 257 °C | 495 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 258 °C @Thickness 3.20 mm |
496 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 253 °C @Thickness 3.20 mm |
487 °F @Thickness 0.126 in |
unannealed; ASTM D648 |