Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow INSPIRE™ D7030EZ Thermoplastic Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INSPIRE™ D7030EZ Thermoplastic Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Filler Content 15 %
15 %
ISO 3451
Melt Flow 27 g/10 min

@Load 2.16 kg,
Temperature 230 °C
27 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ISO 868
Tensile Strength, Yield 24.000 MPa
3480.9 psi
ISO 868
Flexural Modulus 1.8500 GPa
268.32 ksi
ISO 178
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
ISO 180/1A
Falling Dart Impact 33.0 J
24.3 ft-lb
@ 0°C, 6.7 m/s; ASTM D3763
36.0 J
26.6 ft-lb
@ 23°C, 6.7 m/s; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112.0 °C
233.6 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75
Descriptive Properties Value Comments
Five Finger Scratch (N) 10