Mechanical Properties Metric English Comments
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
7.35 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HI100K ABS, High Impact
Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched >= 3.92 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 7.35 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL EI5002 PP
Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical
Izod Impact, Notched >= 3.92 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 7.35 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform..
Izod Impact, Notched >= 3.92 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
>= 7.35 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LUPOY SC1004L PC, High Impact
Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical
Izod Impact, Notched 3.92 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.35 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
7.35 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.92 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.35 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched >= 3.92 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 7.35 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL MC4352 PP+Rubber+MF
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9..
Izod Impact, Notched 3.92 J/cm

@Thickness 6.35 mm
7.35 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 6.35 mm
7.35 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade
High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 6.35 mm
7.35 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 6.35 mm
7.35 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade
High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Temperature 23.0 °C
7.35 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
Izod Impact, Notched 3.92 J/cm

@Thickness 3.20 mm
7.35 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade
High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm
7.35 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy
ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm
7.35 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm
7.35 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron BL60 Impact modifier for PVC
Impact modifier for PVC, White powderInformation provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm
7.35 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Temperature 23.0 °C
7.35 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.92 J/cm

@Temperature -30.0 °C
7.35 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.92 J/cm

@Thickness 3.20 mm
7.35 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade
High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.35 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical MA201 ABS, Low Gloss
Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm
7.35 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron BL60 Impact modifier for PVC
Impact modifier for PVC, White powderInformation provided by Bhansali
Izod Impact, Notched 3.92 J/cm

@Thickness 6.40 mm
7.35 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy
ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali