Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
LNP Lubricomp® LCL-4033 EM Polyetheretherketone, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 |
DSM Akulon® S223-HPG8U (Dry) 43% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ GC1201A-M41 Nylon, Glass Filled and Carbon Filled Reinforced injection grade for conductive applications.Main Features:ConductivityHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D 955 |
MRC Polymers NAXALOY™ 793A7 PC + Polyester Blend • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | 60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4 |
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific) LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA 30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15 Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 4.00 mm |
0.0070 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 4.00 mm |
0.0070 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 GV 30 HW 30% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 4.00 mm |
0.0070 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TR 30 LS nat PA* Product description: Grilamid TR 30 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 LS natural contains a processing a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4164 black 9225 PA*-GF30 Product description: Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TR 55 PA12/MACMI Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Conditioned, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**) Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | |
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | 60x60x2; 290°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |