Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ISO 294-4 |
Polyplastic Armamid® PA GF25-1FR Nylon 6, 25% Glass Fiber Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm @Thickness 2.00 mm |
0.0050 - 0.0090 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**) Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D 955 |
MRC Polymers NAXALOY™ 793A7 PC + Polyester Blend • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | |
LATI Latigray 62-01 CX/75 PA 6 Radiopaque compound based on Polyamide 6 (PA6). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | |
LATI Latigray 82-03 CW/96 F3 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America;.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
LATI Latiohm 62-09 PD01 G/20-V2HF PA6, 20% Glass Fiber Reinforced, Flame Retardant Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties.Availabili.. |
|||
Linear Mold Shrinkage, Transverse | 0.0065 - 0.0090 cm/cm | 0.0065 - 0.0090 in/in | |
LATI Latiohm 80-04 PD01 G/30 PPS, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm @Time 86400 sec |
0.0060 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.0090 cm/cm @Time 86400 sec |
0.0080 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.0090 cm/cm | 0.0080 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6 Description: Glass Reinforced, Toughened Nylon 66/6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFX1717-N1 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66 Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFX1743-N1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6 Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | DIS 294-4 |
Wellman Wellpet® MRGF102-BK1 PET, 35% Mineral/Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |