Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GFX1717-N1 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GFX1717-N1 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Filler Content 43 %
43 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
ISO 527-93
Elongation at Break 3.5 %
3.5 %
ISO 527-93
Flexural Strength 310 MPa
45000 psi
ISO 178-93
Flexural Modulus 11.8 GPa
1710 ksi
ISO 178-93
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-93