Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0080 - 0.0090 cm/cm @Thickness 3.18 mm |
0.0080 - 0.0090 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® PC-30CF/000 BLACK Polycarbonate (PC) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.0090 cm/cm @Thickness 3.18 mm |
0.0080 - 0.0090 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | 60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4 |
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | 60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4 |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
LG Chemical LUPOY GP-1006F General Purpose Modified PC, Unreinforced, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.0095 cm/cm | 0.0080 - 0.0095 in/in | |
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | |
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.020 cm/cm @Time 86400 sec |
0.0080 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 1102 PBT+PC Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.011 cm/cm @Thickness 3.20 mm |
0.0080 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm @Time 86400 sec |
0.0080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm @Time 86400 sec |
0.0080 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC008ESS is a compound based on PA66 resin containing Carbon Fiber. Added features include; Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.011 cm/cm @Time 86400 sec |
0.0080 - 0.011 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm @Thickness 4.00 mm |
0.0080 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4,2577 |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm @Thickness 2.00 mm |
0.0080 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | |
E-Polymers TEKAMID® H12T Unreinforced High Impact PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
BLUESTAR 201G25 PBT, 25% Glass Filled Typical Applications: Energy saving lightingInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
BLUESTAR 403HF-G20 PBT, 20% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4 |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Conditioned, 30% Glass Filled Description: AKROMID B3 GF 30 RM-M natural (3291) is a 30% glass fiber reinforced polyamide 6 with high stiffness and strength, limited moisture absorption and light inherent color.Applications: App.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET) Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |