Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
PolyOne Maxxam™ JN-818.S001-1000 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
PolyOne Maxxam™ PPH-20C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | ASTM D955 |
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO 294-4 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | ASTM D955 |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm @Thickness 3.20 mm |
0.0090 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm @Thickness 3.20 mm |
0.0090 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm @Thickness 3.20 mm |
0.0090 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | |
LATI Latigray 66-01 CX/50 PA 66 Radiopaque compound based on Polyamide 66 (PA66). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | |
LATI Latimass 63-06 D025 PA66 Specific density compound based on Polyamide 66 (PA66). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RAL22 is a compound based on PA66 resin containing PTFE, Aramid Fiber. Added Features: Internally Lubricated |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | mold temp=60°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX905 PPE+PS+PA Automotive. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | mold temp=60°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Time 86400 sec |
0.011 - 0.013 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated Features: Heat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1718-N1 General Purpose Nylon 6 Description: General Purpose Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | on Tensile Bar; E2P method |
Eurostar Staramide AK8 PA66, 40% Mineral Reinforced, Injection Molding Staramide AK8 is a 40% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |