Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 2.34 g/cc
2.34 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113

@Temperature 23.0 °C
113

@Temperature 73.4 °F
ASTM D785
Tensile Strength, Yield 64.1 MPa
9300 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 5.07 GPa
735 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
1.3 mm/min; ASTM D790
Flexural Modulus 4.55 GPa
660 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.530 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched 3.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 194 °C
381 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 271 - 293 °C
520 - 559 °F
Mold Temperature 82.2 - 135 °C
180 - 275 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Appearance Black
Features High Specific Gravity
Non-Toxic
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Appliance Components
Automotive Applications
Consumer Applications
Handles
Industrial Applications
Knobs
Medical/Healthcare Applications
Metal Replacement
Sporting Goods
Weighting & Balancing
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved