| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.011 - 0.020 cm/cm | 0.011 - 0.020 in/in | ASTM D955 |
|
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
|
PolyOne Maxxam™ PPC-20C Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | |
|
Polyplastic Armlen® PP MF 20-2HS-901 Polypropylene, 20% Mineral Filled
Heat stabilized, black colored, HVAC applicationsInformation provided by PolyPlastic Group.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
cm/cm @Thickness 3.17 mm |
0.011
in/in @Thickness 0.125 in |
ASTM D955 |
|
Network Polymers Softflex® 0615
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | 360°C nozzle, 160°C tool; ISO 294-4 |
|
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.015
cm/cm @Thickness 3.20 mm |
0.011
-
0.015
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.013
cm/cm @Thickness 3.20 mm |
0.011
-
0.013
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUPOL HI5204G PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | Test Condition: 150x105x3; 280°C/MT 80°C; 500 bar; acc. ISO 2577 |
|
Ineos ABS Triax® 3158 ABS + Polyamide Blend (DAM), PA66/ABS Pellets (filled)
Triax® 3158 is a PA+ABS-Blend and on-line paintable (195°C). It has very high heat resistance, reduced moisture, improved impact strength, and a low coefficient of linear thermal expansion. It..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.0145 cm/cm | 0.011 - 0.0145 in/in | |
|
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.016 cm/cm | 0.011 - 0.016 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East)
LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
|
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
|
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.020 cm/cm | 0.011 - 0.020 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.014
cm/cm @Thickness 3.20 mm |
0.011
-
0.014
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.014
cm/cm @Thickness 3.20 mm |
0.011
-
0.014
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.014
cm/cm @Thickness 3.20 mm |
0.011
-
0.014
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.014
cm/cm @Thickness 3.20 mm |
0.011
-
0.014
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP Thermocomp PB00A PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PB00A is a compound based on PA 6 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.015
cm/cm @Time 86400 sec |
0.011
-
0.015
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Europe-Africa-Middle East)
High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
|
|||
| Linear Mold Shrinkage, Flow |
0.011
-
0.014
cm/cm @Thickness 3.20 mm |
0.011
-
0.014
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Linear Mold Shrinkage, Flow |
0.011
cm/cm @Thickness 3.00 mm |
0.011
in/in @Thickness 0.118 in |
MD |
|
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo.
|
|||
| Linear Mold Shrinkage, Flow | 0.011 - 0.021 cm/cm | 0.011 - 0.021 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer
Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® BS/2 PA6
Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® L 25 W 40 ESD PA12
Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh..
|
|||
| Linear Mold Shrinkage, Flow |
0.011
cm/cm @Diameter 2.00 mm |
0.011
in/in @Diameter 0.0787 in |
ISO 294-4 |
|
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, Conditioned
Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant..
|
|||
| Linear Mold Shrinkage, Flow |
0.011
cm/cm @Thickness 2.00 mm |
0.011
in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
|
DuPont Performance Polymers Zytel® 70GB30HSL NC010 Nylon 66
Zytel® 70GB30HSL NC010 is a 30% glass bead reinforced heat stabilized polyamide 66 resin.Information provided by DuPont Performance Polymers
|
|||