Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
PolyOne Nymax™ 600 A Zip 43 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® PPC4701 PPC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Thickness 3.17 mm |
0.0070 - 0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2340MHL BK Post Consumer Recycle Nylon 6, 40% Mineral Filled Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.010 cm/cm @Thickness 3.20 mm |
0.0050 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.010 cm/cm @Thickness 3.20 mm |
0.0040 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.010 cm/cm @Thickness 3.20 mm |
0.0040 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.010 cm/cm @Thickness 3.20 mm |
0.0090 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.010 cm/cm @Thickness 3.20 mm |
0.0040 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2156FM PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | |
LATI Laticonther 83 CP/85 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer LNP* LUBRICOMP* KFL36 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific) Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.010 cm/cm @Thickness 3.20 mm |
0.0020 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Thickness 3.20 mm |
0.0070 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.010 cm/cm @Thickness 3.20 mm |
0.0025 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.010 cm/cm @Thickness 4.00 mm |
0.0050 - 0.010 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen HU 30BF4 PP, 30% Bamboo Fiber Filled, Injection Molding Starpylen HU30BF4 is a 30% Bamboo Fiber Reinforced Polypropylene Injection Molding Resin (also known as HU30BF4) (PRELIMINARY DATASHEET)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | ASTM D955 |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ASTM D955 |
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod.. |