SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalate Carbonate
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.19 %

@Time 86400 sec
0.19 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 2.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
2.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 92
92
ASTM D785
Hardness, Rockwell R 127
127
ASTM D785
Tensile Strength at Break 77.0 MPa
11200 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa
9430 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 78 %
78 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.33 GPa
338 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 3.73 J/cm
6.99 ft-lb/in
ASTM D256
Izod Impact, Unnotched 32.04 J/cm
60.02 ft-lb/in
ASTM D4812
Tensile Impact Strength 577 kJ/m²
275 ft-lb/in²
Type S; ASTM D1822
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
Specific Heat Capacity 1.26 J/g-°C
0.301 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 148 °C

@Thickness 3.20 mm
298 °F

@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
Optical Properties Metric English Comments
Refractive Index 1.60
1.60
ASTM D542
Haze 1.0 %

@Thickness 2.54 mm
1.0 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 85 %
85 %
2.54 mm; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity >= 2.50e+17 ohm-cm
>= 2.50e+17 ohm-cm
ASTM D257
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
ASTM D150
3.27

@Frequency 50.0 - 60.0 Hz
3.27

@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in air; ASTM D149
Dissipation Factor 0.0016

@Frequency 50.0 - 60.0 Hz
0.0016

@Frequency 50.0 - 60.0 Hz
ASTM D150
0.026

@Frequency 100 Hz
0.026

@Frequency 100 Hz
ASTM D150
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
15 - 30 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
Descriptive Properties Value Comments
Specific Volume 0.83cm^3/g
ASTM D792