Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm |
0.0030 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm |
0.0030 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** Sorona® FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) formulated to be food c.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | |
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers GPB-130 Polybutylene Terephthalate, 30% Glass Fiber Reinforced Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 G/CF30 L BK 30% GlassCarbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.20 mm |
0.0030 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Time 86400 sec |
0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66 LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFX1624-BK(PTFE) 30% Glass Fiber Reinforced, Lubricated Nylon 66 Description: Glass Fiber Reinforced, Lubricated Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Sim. To ISO 294-4 |
DSM Stanyl® TC155 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 4.00 mm |
0.0030 - 0.0050 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Eurotec |
Eurotec® Tecomid® NB40 GR20 NL XA70 PA6, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm |
0.0030 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT
(Unverified Data**) Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |