Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers GPB-130 Polybutylene Terephthalate, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers GPB-130 Polybutylene Terephthalate, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 124.14 MPa
18005 psi
ASTM D638
Elongation at Break >= 3.0 %
>= 3.0 %
ASTM D638
Flexural Strength 172.41 MPa
25006 psi
ASTM D790
Flexural Modulus 6.483 GPa
940.2 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 157.22 °C
315.00 °F
ASTM D648