Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GFX1624-BK(PTFE) 30% Glass Fiber Reinforced, Lubricated Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GFX1624-BK(PTFE) 30% Glass Fiber Reinforced, Lubricated Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Glass Fiber Reinforced, Lubricated Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Filler Content 30 %
30 %
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ISO 527-93
Elongation at Break 2.4 %
2.4 %
ISO 527-93
Flexural Strength 200 MPa
29000 psi
ISO 178-93
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178-93
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ISO 75-93