Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ASTM D955 |
PolyOne Nymax™ 1280 A HS Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | ASTM D955 |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP1300A(W) PA6, High Viscosity Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | |
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific) LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 7 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 350U PBT (Asia Pacific) Impact modified, UV stabilised, flame retardant polyester with an internal glowwire rating of 850C on 1.6mm flat plaques.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.014 cm/cm @Thickness 3.20 mm |
0.013 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ASTM D955 |
Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content Features: Heat StabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® FRGS25-6-NBK3 25% Glass Sphere Reinforced Flame Retardant Nylon 66 Description: Glass Sphere Reinforced Flame Retardant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6 Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT13-66 XE-NBK1 13% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66 Description: Glass Fiber Reinforced, Toughened, Weatherable Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | DIS 294-4 |
Wellman Wellamid® GS1861-N1(PTFE) Nylon 66, 35% Glass Sphere Reinforced, Enhanced Lubrication All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | DIS 294-4 |
Wellman Wellamid® MR340 42H-NBK1 Nylon 6, 34% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ASTM D955 |
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced Data provided by Clariant Masterbatches |