Polymer Property : Linear Mold Shrinkage, Flow = 0.012 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
PolyOne Maxxam™ PD 2201 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cm
0.0070 - 0.012 in/in
ASTM D955
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™..
Linear Mold Shrinkage, Flow 0.0090 - 0.012 cm/cm
0.0090 - 0.012 in/in
ISO 294-4
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant
Halogen and phosphor freeInformation provided by PolyPlastic Group.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Thickness 3.20 mm
0.010 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved.
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
PolyOne Maxxam™ 34-1520 SSM TFPP Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Linear Mold Shrinkage, Flow 0.011 - 0.012 cm/cm
0.011 - 0.012 in/in
ASTM D955
PolyOne Stat-Tech™ NN-20SS/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cm
0.0070 - 0.012 in/in
ASTM D955
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cm

@Thickness 3.20 mm
0.0070 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cm

@Thickness 3.20 mm
0.0070 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage
Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cm

@Thickness 3.20 mm
0.0070 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL GP3300 PP+MF30%
Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0050 - 0.012 cm/cm

@Thickness 3.20 mm
0.0050 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0050 - 0.012 cm/cm

@Thickness 3.20 mm
0.0050 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® SG3250 PBT+PET+MF25%
Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0050 - 0.012 cm/cm

@Thickness 3.20 mm
0.0050 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® SG3250M PBT+PET+MF25%
Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0090 - 0.012 cm/cm
0.0090 - 0.012 in/in
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Thickness 3.20 mm
0.010 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Linear Mold Shrinkage, Flow 0.0090 - 0.012 cm/cm

@Thickness 3.20 mm
0.0090 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific)
Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Thickness 3.20 mm
0.010 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific)
>PPE+PA66-I-TD10
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East)
>PPE+PA66-I-TD10
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Linear Mold Shrinkage, Flow 0.0030 - 0.012 cm/cm

@Thickness 3.20 mm
0.0030 - 0.012 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® XP-2130A PPS
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ISO DIS 294-4
Wellman Wellamid® GFT13-66 XE-WT1 13% Glass Filled, Toughened Nylon 66
Description: Glass Filled, Toughened Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
DIS 294-4
Wellman Wellamid® GFT1835-WBK1 Nylon 66, 17% Glass Fiber Reinforced, Impact Modified
All information provided by Wellman Engineered Resins.