| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ASTM D792 |
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0800 % | 0.0800 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.30 % | 0.30 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm <br>@Thickness 3.20 mm |
0.0080 - 0.012 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 13 g/10 min <br>@Load 5.00 kg,<br> Temperature 250 °C |
13 g/10 min <br>@Load 11.0 lb,<br> Temperature 482 °F |
ASTM D1238 |
| Melt Index of Compound | 12 g/10 min <br>@Load 5.00 kg,<br> Temperature 250 °C |
12 g/10 min <br>@Load 11.0 lb,<br> Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D638 |
| 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 |
| 49.0 MPa | 7110 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 140 % | 140 % | Type I, 50 mm/min; ASTM D638 |
| 150 % | 150 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 4.0 % | 4.0 % | Type I, 50 mm/min; ASTM D638 |
| 4.0 % | 4.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
| 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 | |
| Flexural Yield Strength | 70.0 MPa | 10200 psi | 2 mm/min; ISO 178 |
| 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 1.92 GPa | 278 ksi | 2 mm/min; ISO 178 |
| 2.00 GPa | 290 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
| 6.00 J/cm <br>@Temperature -30.0 °C |
11.2 ft-lb/in <br>@Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
| 47.0 kJ/m² <br>@Temperature -30.0 °C |
22.4 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 50.0 J <br>@Temperature 23.0 °C |
36.9 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 90.0 µm/m-°C <br>@Temperature -40.0 - 150 °C |
50.0 µin/in-°F <br>@Temperature -40.0 - 302 °F |
ASTM E 831 |
| 90.0 µm/m-°C <br>@Temperature -30.0 - 80.0 °C |
50.0 µin/in-°F <br>@Temperature -22.0 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 95.0 µm/m-°C <br>@Temperature -40.0 - 150 °C |
52.8 µin/in-°F <br>@Temperature -40.0 - 302 °F |
ASTM E 831 |
| 95.0 µm/m-°C <br>@Temperature -30.0 - 80.0 °C |
52.8 µin/in-°F <br>@Temperature -22.0 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C <br>@Thickness 3.20 mm |
210 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 76.0 °C | 169 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 75.0 °C <br>@Thickness 3.20 mm |
167 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
| 117 °C | 243 °F | Rate B/120; ISO 306 | |
| 117 °C | 243 °F | Rate B/50; ASTM D1525 |