| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D 792 |
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 1.1 % | 1.1 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 3.8 % @Temperature 23.0 °C |
3.8 % @Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on tensile bar; SABIC Method |
| 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method | |
| Linear Mold Shrinkage, Transverse | 0.0090 - 0.011 cm/cm @Thickness 3.20 mm |
0.0090 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 280 °C |
15 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
| 20 g/10 min @Load 5.00 kg, Temperature 280 °C |
20 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 60.0 MPa | 8700 psi | Type I, 5 mm/min; ASTM D 638 |
| 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 5 mm/min; ASTM D 638 |
| 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 20 % | 20 % | 50 mm/min; ISO 527 |
| 40 % | 40 % | Type I, 5 mm/min; ASTM D 638 | |
| Elongation at Yield | 4.5 % | 4.5 % | Type I, 5 mm/min; ASTM D 638 |
| 4.5 % | 4.5 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 3.00 GPa | 435 ksi | 5 mm/min; ASTM D 638 |
| 3.10 GPa | 450 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 90.0 MPa | 13100 psi | 2 mm/min; ISO 178 |
| 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| 2.95 GPa | 428 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 | |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
| Charpy Impact, Notched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Impact Test | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 190 °C | 374 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 190 °C @Thickness 3.20 mm |
374 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
| 200 °C | 392 °F | Rate B/120; ISO 306 | |
| 200 °C | 392 °F | Rate B/50; ASTM D 1525 |