Physical Properties Metric English Comments
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Multibase Multi-Flex® TPE A 6221 M BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content
Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Nylene® PA6 Impact Modified 323 HS Nylon 6
Extrusion Grade; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Linear Mold Shrinkage 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
Across Flow; ISO 2577
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Linear Mold Shrinkage 0.013 - 0.016 cm/cm
0.013 - 0.016 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH T15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
Across Flow; ISO 2577
Polykemi AB POLYshine PBT D201 GF20 PBT, Glass Fiber Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.013 - 0.020 cm/cm
0.013 - 0.020 in/in
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Linear Mold Shrinkage 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
ASTM D955
Kolon KOPA® KN126 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Multibase Multi-Flex® A 8502 LC UV RXF/YYWA Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
SK Chemicals SKYPEL M555DH General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
SK Chemicals SKYPEL P128DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
±0.1 after 30 min.; ASTM D1238
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti..
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
After 30 min. at 180°F; ASTM D955
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
±0.1 after 30 min.; ASTM D1238
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti..
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 2.00 mm
0.013 in/in

@Thickness 0.0787 in
Toyobo PELPRENE™ S2001 Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 2.00 mm
0.013 in/in

@Thickness 0.0787 in
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
disk, Injection
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 3.175 mm
0.013 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66
Information provided by A. Schulman.
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 3.175 mm
0.013 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66
Information provided by A. Schulman.
Linear Mold Shrinkage 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
aged 48 hrs at 80; ISO 294
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 3.175 mm
0.013 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6
Information provided by A. Schulman.
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 2.00 mm
0.013 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
Linear Mold Shrinkage 0.013 - 0.016 cm/cm
0.013 - 0.016 in/in
Across Flow; ISO 2577
Polykemi AB POLYfill PPH TS15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 2.00 mm
0.013 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM