Physical Properties Metric English Comments
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
With Flow; ISO 2577
Polykemi AB SCANAMID 66 A52^E Nylon 66, Modified
Information provided by Polykemi AB
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
ASTM D955
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks
Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
ASTM D955
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow
Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Flow
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Transverse
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Plastcom SLOVALEN PC 93 T 30 PP reinforced with 30% mineral filler
Features: Modified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furni..
Linear Mold Shrinkage 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ASTM D955
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Linear Mold Shrinkage 0.016 - 0.025 cm/cm
0.016 - 0.025 in/in
FRISETTA Test Method
Nilit FRIANYL B63 ND Nylon 6
Nylon 6, low viscosity, permanently flexible, dry impact resistant (dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer  (Unverified Data**)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
Lehmann & Voss LUVOCOM® 80-7318 Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Linear Mold Shrinkage 0.016 - 0.019 cm/cm
0.016 - 0.019 in/in
ASTM D955
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Global PPC-0320 Standard Grade Polypropylene
Information provided by Global Polymers Corporation.
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Ineos 3950 Polypropylene Impact Copolymer
Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Tool, Montell
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant
Key Features: medium melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colorability..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
LyondellBasell Hifaxâ„¢ AA36H Polypropylene Homopolymer
Description: Hifaxâ„¢ AA36H conventional melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabi..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Teknor Apex Monprene® MP-2228 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Teknor Apex Monprene® MP-1389E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Tipco Tipcolene® FPC 20 HG - 20% Calcium Carbonate Reinforced, High Gloss Polypropylene Homopolymer
20% Calcium Carbonate Filled PP Homopolymer with High GlossApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Tipco Tipcolene® PPC FR V0 - UL94-V0 Flame Retardant Polypropylene Copolymer
V-0 Flame Retardant PP CopolymerApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Linear Mold Shrinkage 0.016 - 0.026 cm/cm
0.016 - 0.026 in/in
ASTM D955
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer
Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons..
Linear Mold Shrinkage 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
Asahi Kasei Method
Asahi Kasei Tenac®-C 5520 Copolymer Acetal Resin
Similar to TENAC®-C 4520 but with higher flow and minimized mold deposit.Information provided by Asahi Kasei Corporation.
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
A. Schulman ComAlloy Lubrilon® 640 Nylon 6/12, PTFE Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Aaron Industries AAROPRENE® AEN 6600-3 Nylon 6/6 Engineered Resin
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound
PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Linear Mold Shrinkage 0.016 - 0.019 cm/cm
0.016 - 0.019 in/in
ISO 2577
Polyram RamSter PF801 PBT, High Impact Modified
High impact modified PBT for injection molding applications.Information provided by Polyram.