| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage |
0.017
-
0.020
cm/cm <br>@Thickness 3.17 mm
|
0.017
-
0.020
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Network Polymers Softflex® 0809
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
|
|||
| Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 TF30 Nylon 6.6 for injection molding, 30% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYshine PBT D201 PBT
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.012 - 0.020 cm/cm | 0.012 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 KV25 Nylon 6.6 for injection molding, 25% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage |
0.010
-
0.020
cm/cm <br>@Thickness 3.17 mm
|
0.010
-
0.020
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
PolyOne Lubri-Tech™ NL-000/40T Nylon 6/12 - 40% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
|
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding
Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f..
|
|||
| Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
|
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer
BorPure™ RE450MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is characterized by optimum combination of high impact strength and..
|
|||
| Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
|
Borealis HH315MO Polypropylene
HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec..
|
|||
| Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
|
Borealis MG9621B Polyethylene
Applications: crates, and pailsInformation provided by Borealis AG
|
|||
| Linear Mold Shrinkage | 0.0020 - 0.020 cm/cm | 0.0020 - 0.020 in/in | ASTM D955 |
|
Cheng Yu Plastic N66C2 Nylon 66, 20% Mineral Reinforced |
|||
| Linear Mold Shrinkage | 0.0020 - 0.020 cm/cm | 0.0020 - 0.020 in/in | ASTM D955 |
|
Cheng Yu Plastic NG1300S Nylon 66, 30% Glass Fiber Reinforced |
|||
| Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
|
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber |
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 502700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 600350S SEBS Based Material, Filled Qualities, 35A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 602350S SEBS Based Material, Filled Qualities, 35A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 602600S SEBS Based Material, Filled Qualities, 60A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 660300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
|
ELASTO UK Dryflex® 660750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
|
CPT C-Flex® R70-214 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
|
Chang Chun Plastic PBT1200M General Purpose PBT
Information provided by Dowell Trading Company Ltd.
|
|||
| Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
|
Cheng Yu Plastic FV3025 Polyformaldehyde |
|||
| Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
|
Beijing Chemical Industry KAIFA® HN201-G0 PA6 Resin
Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
|
Cheng Yu Plastic FV30BK Electric Conducting Polyformaldehyde |
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
|
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
|
Beijing Ranger Chem PBT-201-G0 211 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||