Polymer Property : Linear Mold Shrinkage = 0.022 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D955-89
Multibase Multi-Pro® 0110 X Natural Polypropylene
This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide..
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
With Flow; ISO 2577
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0050 - 0.022 cm/cm
0.0050 - 0.022 in/in
FRISETTA Test Method
Nilit FRIANYL A63 W-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.012 - 0.022 cm/cm
0.012 - 0.022 in/in
FRISETTA Test Method
Nilit FRIANYL B63 S20 Nylon 6 for injection molding
Nylon 6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.014 - 0.022 cm/cm
0.014 - 0.022 in/in
FRISETTA Test Method
Nilit RECONYL B S Recycled nylon 6 for injection molding
Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D955
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
ASTM D955
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified
Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Asahi Chemical test
Asahi Kasei Tenac® FA405 Acetal Homopolymer, Low Friction Grade  (discontinued **)
Contains fluoropolymer and lubricant; excellent friction and wear on plastics.Applications: Bearings for printers, cams, gears.This product is not a part of the standard product line dated 2003.
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
Lehmann & Voss LUVOCOM® 80/TF/18/GY Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
Lehmann & Voss LUVOCOM® 80-7318 Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Linear Mold Shrinkage 0.014 - 0.022 cm/cm

@Thickness 3.00 mm
0.014 - 0.022 in/in

@Thickness 0.118 in
ASTM D955
Samyang Tribit® 1503 Polybutylene Terephthalate
Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid..
Linear Mold Shrinkage 0.014 - 0.022 cm/cm

@Thickness 3.00 mm
0.014 - 0.022 in/in

@Thickness 0.118 in
ASTM D955
Samyang Tribit® 1503S Polybutylene Terephthalate
Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Polyram RamTal PM1109 Acetal, General Purpose
General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Polyram RamTal PM7002 Acetal, UV Stabilized
UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Polyram RamTal PM7109 Acetal, UV Stabilized
UV stabilized polyacetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO 2577
Polyram RamTal PMH2003 Polyacetal Homopolymer for Injection Molding
General purpose polyacetal homopolymer for injection molding applications, MFI 3.Information provided by Polyram.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO 2577
Polyram RamTal PMH2010 Polyacetal Homopolymer for Injection Molding
General purpose polyacetal homopolymer for injection molding applications, MFI 10.Information provided by Polyram.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Polyram RamTal PM1409 Acetal, PTFE Filled
Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
ASTM D955
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
ASTM D955
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.012 - 0.022 cm/cm
0.012 - 0.022 in/in
ASTM D955
Beijing Chemical Industry KAIFA® 101 PBT Resin
Unreinforced, good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Asahi Kasei Method
Asahi Kasei Tenac® 3013A Homopolymer Acetal Resin
Weather-Resistant grade containing UV absorber and other additives for superior weathering abilityInformation provided by Asahi Kasei Corporation.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Asahi Kasei Method
Asahi Kasei Tenac® 4010 Homopolymer Acetal Resin
General purpose grade, high impact, high elongation, medium viscosityInformation provided by Asahi Kasei Corporation.
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Asahi Kasei Method
Asahi Kasei Tenac® LA543 Homopolymer Acetal Resin
Excellent friction and wear on metals and plastics, except POM.Information provided by Asahi Kasei Corporation.
Linear Mold Shrinkage 0.012 - 0.022 cm/cm
0.012 - 0.022 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound
PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P..
Linear Mold Shrinkage 0.016 - 0.022 cm/cm
0.016 - 0.022 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound
PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..