Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of products of Kocetal are short term: 140-150C and long term: 100-120C.Mechanical Properties: Kocetal is an engineering plastic that has excellent strength, stiffness and wear endurance. Also, it offers an excellent balance of several properties. For example, mechanical properties are stable in the practical temperature zone (-50C to 80C), compared to Nylon and PBT resins. Although it has slightly lower initial strength, compared to homopolymer, the long term properties of "elongation at break and impact strength" are superior.Electrical Properties: Kocetal has excellent electrical properties. Its electrical properties, volume resistivity, dielectric constant, dissipation factor and dielectric strength change little with temperature. It also has a feature of good anti-pollution properties on electrical contact. Kocetal has such a permanent anti-static grade that can be applied to the specifics.Chemical Properties: Kocetal has excellent chemical resistance to organic chemicals, oils, fats and detergents. It is also strongly resistant to inorganic chemicals except strong acids.Information provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D790
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 83
83
ASTM D785
Tensile Strength, Ultimate 58.8 MPa
8530 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Yield Strength 98.1 MPa
14200 psi
ASTM D790
Flexural Modulus 4.90 GPa
711 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.0 - 70.0 µm/m-°C

@Temperature 20.0 °C
27.8 - 38.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 166 °C
331 °F
ASTM D1525
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
Long Term
140 - 150 °C
284 - 302 °F
Short Term
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149