Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos 3950 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos 3950 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsAutomotive interior trimBenefitsLow glossHigh impact resistance
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790B
Izod Impact, Notched 1.33 J/cm

@Diameter 3.17 mm
2.50 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
0.481 J/cm

@Diameter 3.00 mm,
Temperature -20.0 °C
0.900 ft-lb/in

@Diameter 0.118 in,
Temperature -4.00 °F
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
ASTM D648
Flame Spread 27.5 mm/min
1.08 in/min
FMVSS 302
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: