Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.36 g/cc | 0.0491 lb/in³ | |
Plastcom SLOVAMID 66 GB 30 LS PA66, 30% glass beads, light stability Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ±0.03 g/cm³; DIN 53479 |
PolyOne Bergamid™ B65 G30 black IG Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO data |
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | DIN 53479 |
Qualchem Danamid FGFHUV-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial light.Information provided by Qualchem Zrt. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183/A |
Solvay TECHNYL® R CR 218 V30 Nylon 6, 30% glass fiber, DRY TECHNYL® CR 218 V30 is a polyamide 6, reinforced with 30% glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color.Benefit.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East) LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6 GF15 TL15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6 LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RX06027 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RX06027 is a compound based on PA 66 containing Glass Bead. Added features include: Easy Molding, Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | |
Goodfellow Polyethylene Naphthalate (PEN) Film A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colo.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S223-HG6 (Cond.) 30% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Aclo Accutech ABS ABS833G40L Glass Reinforced |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183-1-A |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Information provided by BASF |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183/A |
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL32XXP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1138 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |