Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183-1 |
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data) Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro.. |
|||
Density | 1.29 - 1.62 g/cc | 0.0466 - 0.0585 lb/in³ | Average value: 1.41 g/cc Grade Count:17 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
PolyOne Stat-Tech™ PI-05CF/000 Polyetherimide - 5% Carbon Fibers - ESD Applications
(discontinued **) Data provided by PolyOne. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | |
Lord Adhesives HPC-6B Ethylene Acrylic Elastomer Coating LORD HPC-6B and HPC-6C are one-part, room temperature curing ethylene acrylic elastomer (AEM) coatings which feature robust adhesion and exceptional mechanical properties. These coatings enhance ozo.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
Lanxess Pocan® B 1505 Z 000000 PBT PBT, non-reinforced, injection molding, extrusion, impact modified |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific) LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific) LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon DEF13 PC LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Toyobo PELPRENE™ S9001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TSGZ-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | JIS-Z-8807 |
Denka REOMER G G5072 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
BASF Ultramid® C3U10 PA6/66 FR (Conditioned) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® P114 PBT Polyester A high impact polyester with low shrinkage.Data provided by the manufacturer |
|||
Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 95/3 Flexible PVC, Insulation for High Temperatures Lead Free Operating temperature 90°C |