Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Westlake Plastics
Trade Name Zelux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 0.18 %
0.18 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
ASTM D2240
Tensile Strength, Yield 65.5 MPa
9500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.231 W/m-K
1.60 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.508 mm
V-0

@Thickness 0.0200 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 - 1.00e+11 ohm-cm
1.00e+7 - 1.00e+11 ohm-cm
Dry; ASTM D257
Surface Resistance 1.00e+7 - 1.00e+11 ohm
1.00e+7 - 1.00e+11 ohm
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B