Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9320 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9410 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum Modified PPO - Noryl® Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | >= 0.231 W/m-K | >= 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Edgetek® AS-30GF/000 FRVO Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Thermal Conductivity | 0.231 - 0.288 W/m-K | 1.60 - 2.00 BTU-in/hr-ft²-°F | Average value: 0.269 W/m-K Grade Count:3 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
ScanTube ETFE Tubing Information provided by ScanTube, Inc. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Pomalux® Acetal Copolymer Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Thermal Conductivity | 0.231 - 0.245 W/m-K | 1.60 - 1.70 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:4 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.231 - 0.403 W/m-K | 1.60 - 2.80 BTU-in/hr-ft²-°F | Average value: 0.323 W/m-K Grade Count:5 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Thermal Conductivity | >= 0.231 W/m-K | >= 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |