Buckeye Polymers BP FLEX D5512 RU BLK Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D5512 RU BLK Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Melt Flow 10 - 14 g/10 min
10 - 14 g/10 min
ASTM D1238
Ash 0.00 - 5.0 %
0.00 - 5.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 10.1 MPa
>= 1470 psi
ASTM D638
Flexural Modulus 0.4699 - 0.94975 GPa
68.15 - 137.75 ksi
ASTM D790
Izod Impact, Notched >= 2.14 J/cm
>= 4.00 ft-lb/in
ASTM D256