Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable

Category Ceramic , Carbide , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name VIBRON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, this material has a very good resistance against several aggressive slags.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.45 - 2.55 g/cc
0.0885 - 0.0921 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 80.0 - 90.0 MPa

@Temperature 100 °C
11600 - 13100 psi

@Temperature 212 °F
Cold Crushing Strength
95.0 - 105 MPa

@Temperature 1400 °C
13800 - 15200 psi

@Temperature 2550 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.35 - 1.55 W/m-K

@Temperature 100 °C
9.37 - 10.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.45 - 1.65 W/m-K

@Temperature 600 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.51 - 1.71 W/m-K

@Temperature 1400 °C
10.5 - 11.9 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1400 °C
-0.200 - 0.200 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 54 %
54 %
Fe2O3 1.0 %
1.0 %
SiC 9.0 %
9.0 %
SiO2 31 %
31 %
Descriptive Properties Value Comments
ASTM Classification Class E
Material Consumption per 1 m3 2450 kg
Mixing Water 4.5-5.5 liters
per 100 kgs dry material
Users viewing this material also viewed the following: