Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled

Category Polymer , Film , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name APTIV®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK 1100 has a unique combination of properties providing high temperature performance, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen free and ease of processing makes APTIV films a technology enabler for our customers and end users. APTIV PEEK 1100 series provides a higher modulus and lower coefficient of linear thermal expansion over the APTIV 1000 series.Applications:Electrical InsulationPrinted circuit substratesHigh temperature labelsFlexible surface heatersPressure sensor membranesAcoustic speaker diaphragms and voice coilsProven temperature resistance to use of lead free soldersAPTIV film is FDA and EU approved for food contact and is RoHS compliant.All information provided by Victrex.Property data reported herein was measured on 50 micron film. The films are available in thicknesses from 12 microns up to 125 microns.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc

@Temperature 23.0 °C
1.45 g/cc

@Temperature 73.4 °F
ISO 1183
Moisture Absorption at Equilibrium 0.080 %

@Temperature 23.0 °C,
Time 86400 sec
0.080 %

@Temperature 73.4 °F,
Time 24.0 hour
50% RH; ISO 62
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 100 %
>= 100 %
ISO 527
>= 100 %

@Thickness 0.0250 mm
>= 100 %

@Thickness 0.000984 in
ISO 527
>= 100 %

@Thickness 0.0250 mm
>= 100 %

@Thickness 0.000984 in
ISO 527
Film Elongation at Break, TD >= 10 %
>= 10 %
ISO 527
>= 10 %

@Thickness 0.100 mm
>= 10 %

@Thickness 0.00394 in
ISO 527
>= 10 %

@Thickness 0.100 mm
>= 10 %

@Thickness 0.00394 in
ISO 527
Tensile Modulus 4.30 GPa
624 ksi
TD; ISO 527
4.80 GPa
696 ksi
MD; ISO 527
4.20 GPa

@Thickness 0.100 mm
609 ksi

@Thickness 0.00394 in
TD; ISO 527
4.50 GPa

@Thickness 0.0250 mm
653 ksi

@Thickness 0.000984 in
TD; ISO 527
4.50 GPa

@Thickness 0.100 mm
653 ksi

@Thickness 0.00394 in
MD; ISO 527
5.00 GPa

@Thickness 0.0250 mm
725 ksi

@Thickness 0.000984 in
MD; ISO 527
Tear Strength 5.96 kN/m
34.0 pli
MD; ISO 6383-1
6.84 kN/m
39.0 pli
TD; ISO 6383-1
Film Tensile Strength at Break, MD 100 MPa
14500 psi
ISO 527
100 MPa

@Thickness 0.0250 mm
14500 psi

@Thickness 0.000984 in
ISO 527
100 MPa

@Thickness 0.100 mm
14500 psi

@Thickness 0.00394 in
ISO 527
Film Tensile Strength at Break, TD 80.0 MPa
11600 psi
ISO 527
80.0 MPa

@Thickness 0.0250 mm
11600 psi

@Thickness 0.000984 in
ISO 527
80.0 MPa

@Thickness 0.100 mm
11600 psi

@Thickness 0.00394 in
ISO 527
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C
19.4 µin/in-°F
MD, below Tg; ASTM D696
Thermal Conductivity 0.430 W/m-K
2.98 BTU-in/hr-ft²-°F
Through Plane; ASTM E1461
0.910 W/m-K
6.32 BTU-in/hr-ft²-°F
In-Plane; ASTM E1461
Shrinkage, MD <= 0.50 %

@Temperature 200 °C
<= 0.50 %

@Temperature 392 °F
TM-XV-84
Shrinkage, TD <= 0.50 %

@Temperature 200 °C
<= 0.50 %

@Temperature 392 °F
TM-XV-84
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
100V; ASTM D257
Dielectric Constant 3.6

@Frequency 1e+7 Hz,
Temperature 23.0 °C
3.6

@Frequency 1e+7 Hz,
Temperature 73.4 °F
Dielectric Strength 200 kV/mm

@Temperature 23.0 °C
5080 kV/in

@Temperature 73.4 °F
1/4 inch electrode; ASTM D149
Dissipation Factor 0.0010

@Frequency 1e+7 Hz,
Temperature 23.0 °C
0.0010

@Frequency 1e+7 Hz,
Temperature 73.4 °F
ASTM D150
Descriptive Properties Value Comments
Puncture Strength 5 kJ/m²
MD/TD, Def Stan 81-75; 23°C